严寒区浮石混凝土分级评价与孔结构响应阈值
CSTR:
作者:
作者单位:

1.内蒙古工业大学 土木工程学院,内蒙古 呼和浩特 010051;2.内蒙古工业大学 内蒙古自治区土木工程绿色建造与智能运维重点实验室,内蒙古 呼和浩特 010051;3.内蒙古工业大学 资源与环境工程学院,内蒙古 呼和浩特 010051;4.内蒙古工业大学 生态型建筑材料与装配式结构内蒙古自治区工程研究中心,内蒙古 呼和浩特 010051

作者简介:

王萧萧(1987—),女,山东济宁人,内蒙古工业大学副教授,硕士生导师,博士。E-mail:wxiaoxiao.good@163.com

通讯作者:

闫长旺(1978—),男,内蒙古包头人,内蒙古工业大学教授,博士生导师,博士。E-mail:ycw20031013@126.com

中图分类号:

TU528.2

基金项目:

国家自然科学基金资助项目(52469023,52068059,52368036);内蒙古科技计划项目(2022YFDZ0023,2023YFDZ0049);中央引导地方科技发展资金2022ZY0160;鄂尔多斯市重点研发计划(YF20232358);呼伦贝尔市“科技兴市”行动重点项目(2023HZZX007)


Classification Evaluation and Response Threshold of Pore Structure of Pumice Concrete in Cold Regions
Author:
Affiliation:

1.School of Civil Engineering, Inner Mongolia University of Technology, Hohhot 010051, China;2.Inner Mongolia Key Laboratory of Green Construction and Intelligent Operation and Maintenance of Civil Engineering, Inner Mongolia University of Technology, Hohhot 010051, China;3.School of Resources and Environmental Engineering, Inner Mongolia University of Technology, Hohhot 010051, China;4.Inner Mongolia Engineering Research Center for Ecological Building Materials and Prefabricated Structures, Inner Mongolia University of Technology, Hohhot 010051, China

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    基于浮石混凝土(PAC)的孔隙率、孔径分布和分形维数计算增益系数(Ygp)、损伤系数(Cgp)。利用阈值指标分类法得到PAC的水化程度、损伤程度各阶段临界点,根据分级评价和宏观性能确定PAC孔结构的增益阈值与损伤阈值。结果表明:0.947<Ygp1.000为充分水化、0.927<Ygp0.947为一般水化、0.912Ygp0.927为不良水化;1.00Cgp1.07为轻微损伤、1.07<Cgp1.16为中度损伤、1.16<Cgp1.51为严重损伤。该研究为严寒区浮石混凝土水化程度和损伤程度的分级、定量评价提供了方法。

    Abstract:

    Gain coefficient(Ygp) and damage coefficient(Cgp) were calculated based on the porosity, pore size distribution and fractal dimension of pumice concrete. The critical points of hydration degree and damage degree were obtained through the classification of threshold index, and the gain threshold and damage threshold were determined according to the classification evaluation and macro performance. The results show that 0.947<Ygp≤1.000 indicates adequate hydration, 0.927<Ygp≤0.947 indicates average hydration, and 0.912≤Ygp≤0.927 indicates poor hydration. 1.00≤Cgp≤1.07 indicates minor injury, 1.07<Cgp≤1.16 indicates moderate injury, and 1.16<Cgp≤1.51 indicates severe injury. This work provides a method for grading and quantitative evaluation of hydration degree and damage degree of pumice concrete in cold regions.

    参考文献
    相似文献
    引证文献
引用本文

王萧萧,董培森,闫长旺,刘曙光,张菊.严寒区浮石混凝土分级评价与孔结构响应阈值[J].建筑材料学报,2025,28(6):526-535

复制
相关视频

分享
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2024-09-12
  • 最后修改日期:2024-12-11
  • 录用日期:
  • 在线发布日期: 2025-06-29
  • 出版日期:
文章二维码